To begin volume/composite testing, shredded paper and few plastic bits turned and mashed in water, spread in plastic bin where fast acting Durabond mix was added and a bottle was positioned. Hardening and separation from mould was achieved within 35min for portions 1" thick. Silicone helped only slightly in removing rock from metal flashing.